<?xml version="1.0" encoding="UTF-8"?>
<rdf:RDF xmlns="http://purl.org/rss/1.0/" xmlns:rdf="http://www.w3.org/1999/02/22-rdf-syntax-ns#" xmlns:dc="http://purl.org/dc/elements/1.1/">
<channel rdf:about="http://dspace.nbuv.gov.ua:80/handle/123456789/71022">
<title>Наносистеми, наноматеріали, нанотехнології, 2013, № 3</title>
<link>http://dspace.nbuv.gov.ua:80/handle/123456789/71022</link>
<description/>
<items>
<rdf:Seq>
<rdf:li rdf:resource="http://dspace.nbuv.gov.ua:80/handle/123456789/75918"/>
<rdf:li rdf:resource="http://dspace.nbuv.gov.ua:80/handle/123456789/75917"/>
<rdf:li rdf:resource="http://dspace.nbuv.gov.ua:80/handle/123456789/75916"/>
<rdf:li rdf:resource="http://dspace.nbuv.gov.ua:80/handle/123456789/75915"/>
</rdf:Seq>
</items>
<dc:date>2026-04-04T20:14:26Z</dc:date>
</channel>
<item rdf:about="http://dspace.nbuv.gov.ua:80/handle/123456789/75918">
<title>Загальні закономірності та особливості утворення біонанокомпозитів ароматичних амінокислот з багатошаровими вуглецевими нанорурками</title>
<link>http://dspace.nbuv.gov.ua:80/handle/123456789/75918</link>
<description>Загальні закономірності та особливості утворення біонанокомпозитів ароматичних амінокислот з багатошаровими вуглецевими нанорурками
Маніло, М.В.; Ар’єв, І.А.; Литвинов, Г.С.
Експериментально досліджено та проаналізовано впливи експозиції, концентрацій, рН і структури ароматичних амінокислот на їх адсорбцію багатошаровими вуглецевими нанорурками. Одержано основні кількісні характеристики взаємодії амінокислот з вуглецевими нанорурками (константи&#13;
швидкости, величини адсорбції, Ґіббсові вільні енергії, посадкові майданчики молекул), побудовано кінетичні криві та ізотерми іммобілізації.&#13;
Виявлено, що для всіх досліджених ароматичних амінокислот спостерігається унікальний дзвоноподібний максимум адсорбції в околі рН 6,0, а&#13;
детальні параметри кінетики процесу іммобілізації, ізотерми, кількість&#13;
та посадкові майданчики молекул адсорбату на поверхні вуглецевих нанорурок виявилися індивідуальними для різних амінокислот.; Экспериментально исследованы и проанализированы влияния экспозиций,&#13;
концентраций, рН и структуры ароматических аминокислот на их адсорбцию многослойными углеродными нанотрубками. Получены основные количественные характеристики взаимодействия аминокислот с углеродными&#13;
нанотрубками (константы скорости, величины адсорбции, свободные энергии Гиббса, посадочные площадки молекул), построены кинетические кривые и изотермы иммобилизации. Установлено, что для всех исследованных&#13;
ароматических аминокислот одиночный колоколообразный максимум адсорбции наблюдается в окрестности рН 6,0. Детальные параметры кинетики&#13;
процесса иммобилизации, изотермы, количество и посадочные площадки молекул адсорбата на поверхности углеродных нанотрубок оказались индивидуальными для разных аминокислот.; Influences of exposure, concentration, pH, and structure of aromatic amino&#13;
acids on adsorption of them by multiwalled carbon nanotubes are investigat-ed and analysed. Fundamental quantity characteristics of the amino acid interaction&#13;
with the carbon nanotubes (such as rate constant, adsorption degree,&#13;
Gibbs free energies, attachment-pad areas per molecule are obtained.&#13;
Based on the experimental data, kinetic curves and isotherms of immobilization&#13;
are plotted. As found for the studied amino acids, there is a unique belllike&#13;
maximum of adsorption near 6.0 pH, but the detailed parameters of the&#13;
immobilization kinetics, isotherms, molecules’ quantity, and an area per adsorbed&#13;
molecule are individual for each amino acid.
</description>
<dc:date>2013-01-01T00:00:00Z</dc:date>
</item>
<item rdf:about="http://dspace.nbuv.gov.ua:80/handle/123456789/75917">
<title>Одержання гібридних нанокристалів з використанням наномагнетиту та наночастинок Ag у водних розчинах</title>
<link>http://dspace.nbuv.gov.ua:80/handle/123456789/75917</link>
<description>Одержання гібридних нанокристалів з використанням наномагнетиту та наночастинок Ag у водних розчинах
Кравцова, А.С.; Коров’янко, О.О.; Стратійчук, І.Б.; Буркут, В.І.
В роботі представлено методу синтезу гібридних наносистем на основі наночастинок срібла та магнетиту. Досліджено вплив системи відновників на процес формування та швидкість утворення наночастинок срібла, вплив природи желатину на їх морфологію, стабільність розчинів у часі та інтенсивність плазмового резонансу. Запропоновано альтернативні методи відновлення солей арґентуму алкалоїдами — галовою кислотою та пірокатехіновим альдегідом. Показано можливість одержання стабільних колоїдних розчинів гетероструктур нанокристалів оксиду заліза та плазмового металу складу Fe₃O₄–Ag.; A given paper presents a method for synthesis of hybrid nanosystems based on silver nanoparticles and magnetite. The influence of reductants on both the formation and the forming rate of silver nanoparticles, the effect of gelatine nature on their morphology, stability of solutions in time, and intensity of the plasmon resonance are investigated. Alternative methods of argentum salts recovering by such alkaloids as gallic acid and pyrocatechin aldehyde are proposed. The possibility of fabrication of the stable colloid solutions of heterostructures based on the iron oxide and plasmon metal (Fe₃O₄–Ag) nanocrystals is shown.; В работе представлен метод синтеза гибридных наносистем на основе наночастиц серебра и магнетита. Исследовано влияние системы восстановителей на процесс формирования и скорость образования наночастиц серебра, влияние природы желатина на их морфологию, стабильность растворов во времени и интенсивность плазменного резонанса. Предложены альтернативные методы восстановления солей серебра алкалоидами — галловой кислотой и пирокатехиновым альдегидом. Показана возможность получения стабильных коллоидных растворов гетероструктурнанокристаллов оксида железа и плазменного металла состава Fe₃O₄–Ag.
</description>
<dc:date>2013-01-01T00:00:00Z</dc:date>
</item>
<item rdf:about="http://dspace.nbuv.gov.ua:80/handle/123456789/75916">
<title>Effect of High-Pressure Treatment on Structure and Properties of Invar Fe–35% Ni Alloy</title>
<link>http://dspace.nbuv.gov.ua:80/handle/123456789/75916</link>
<description>Effect of High-Pressure Treatment on Structure and Properties of Invar Fe–35% Ni Alloy
Nadutov, V.M.; Vashchuk, D.L.; Volosevich, P.Yu.; Beloshenko, V.A.; Spuskanyuk, V.Z.; Davidenko, O.A.
The effect of uniform high-pressure (HP) treatment on change of the internal structure hierarchy of polycrystalline Invar f.c.c. Fe–35.0% Ni alloy in quenched state and after hydroextrusion (HE) is studied. As shown, the treatment of the quenched alloy by pressure of 2 GPa is accompanied by the relief formation on the cross-section surface that is caused by reorientation of available grains and by a change of grain-boundaries’ state. The increase of density of twins of deformation and the saturation of structural elements by vacancies and dislocations promoting the grain-boundary slipping is revealed. The HP processing of the previously HE treated samples of the Invar alloy (ε =0.96 and 1.12) is not accompanied by notable distinctions in the structures’ hierarchy with the exception of both the decrease of texture and the increase of twins’ density that is caused by partial stress relaxation.; Досліджено вплив оброблення всебічним тиском (ВТ) на зміну структурної ієрархії полікристалічного інварного стопу ГЦК-Fe–35,0% Ni в загартованому стані, а також після оброблення гідроекструзією (ГЕ). Показано, що оброблення тиском у 2 ГПа стопу в загартованому стані супроводжується формуванням на поверхнях шліфа рельєфу, що обумовлено переорієнтацією в просторі зерен і зміною стану їх меж. Виявлено збільшення густини двійників деформації і насичення структурних елементів вакансіями та дислокаціями, які сприяють зерномежовому проковзуванню. Оброблення ВТ попередньо деформованих гідроекструзією зразків інварного стопу (ε = 0,96 і 1,12) не супроводжується помітними відмінностями в ієрархії структури, за винятком зменшення текстури і збільшення густини двійників, що є результатом часткової релаксації мікронапружень.; Исследовано влияние обработки всесторонним давлением (ВД) на изменение структурной иерархии поликристаллического инварного сплава ГЦК- Fe–35,0% Ni в закалённом состоянии, а также после обработки гидроэкструзией (ГЭ). Показано, что обработка давлением в 2 ГПа сплава в закалённом состоянии сопровождается формированием на поверхностях шлифов рельефа, обусловленного переориентацией в пространстве зёрен и изменением состояния их границ. Обнаружено увеличение плотности двойников деформации и насыщение структурных элементов вакансиями и дислокациями, способствующими зернограничному проскальзыванию. Обработка ВД предварительно обработанных гидроэкструзией образцов инварного сплава (ε = 0,96 и 1,12) не сопровождается заметными различиями в иерархии структуры, за исключением уменьшения текстуры и увеличения плотности двойников, являющихся результатом частичной релаксации микронапряжений.
</description>
<dc:date>2013-01-01T00:00:00Z</dc:date>
</item>
<item rdf:about="http://dspace.nbuv.gov.ua:80/handle/123456789/75915">
<title>Influence of Ultrasonic Treatment of Activated Carbon in Cavitation and Precavitation Regimes on Capacitive and Pseudocapacitive Energy Storage in Electrochemical Supercapacitors</title>
<link>http://dspace.nbuv.gov.ua:80/handle/123456789/75915</link>
<description>Influence of Ultrasonic Treatment of Activated Carbon in Cavitation and Precavitation Regimes on Capacitive and Pseudocapacitive Energy Storage in Electrochemical Supercapacitors
Influence of ultrasonic treatment of activated carbon on the electric double&#13;
layer in interface between the carbon and the 7.6 m KOН, 4 m KI, and 2 m&#13;
ZnI2 aqueous electrolyte solutions as well as on the working parameters of&#13;
supercapacitors on their base is studied by means of precision porometry,&#13;
small angle X-ray scattering, cyclic voltamperometry, electrochemical impedance&#13;
spectroscopy, and computer simulation methods. As shown, the ultrasonic&#13;
treatment at precavitation regimes causes the significant (more&#13;
than by 200 times) increase of density of states at the Fermi level that is the&#13;
reason not only quantitative but also qualitative changes in farad–volt dependences.&#13;
At the same time, an acoustic cavitation field unblocks the Helmholtz&#13;
capacitance due to large decrease of volume-charge-region resistance.&#13;
Using these data, we propose the new electrochemical system of functionalhybrid&#13;
supercapacitor with specific capacitance 1100 F/g and specific energy&#13;
49 W·h/kg.; За допомогою прецизійної порометрії, малокутового Рентґенового розсіяння, циклічної вольтамперометрії, електрохемічної імпедансної спектроскопії та комп’ютерного моделювання досліджено вплив ультразвукового оброблення активованого вугілля на параметри подвійного електричного шару межі поділу його з водними розчинами електролітів&#13;
7,6 m KOH, 4 m KI і 2 m ZnI2 та експлуатаційні характеристики суперконденсаторів на їх основі. Показано, що ультразвукове оброблення докавітаційними режимами призводить до значного (більше ніж у 200 разів)&#13;
збільшення густини станів на рівні Фермі, що призводить не тільки до&#13;
кількісних, але і до якісних змін вольт-фарадних залежностей. В той же&#13;
час вплив поля акустичної кавітації деблокує Гельмгольцову місткість за&#13;
рахунок сильного зменшення опору области просторового заряду в твердому тілі. На основі одержаних даних розроблено електрохемічну систему&#13;
гібридного суперконденсатора з питомою місткістю у 1100 Ф/г і питомою&#13;
енергією у 49 Втгод/кг.; С помощью прецизионной порометрии, малоуглового рентгеновского рассеяния, циклической вольтамперометрии, электрохимической импедансной спектроскопии и компьютерного моделирования исследовано&#13;
влияние ультразвуковой обработки активированного угля на параметры&#13;
двойного электрического слоя границы его раздела с водными растворами&#13;
электролитов 7,6 m KOH, 4 m KI и 2 m ZnI2 и эксплуатационные характеристики суперконденсаторов на их основе. Показано, что ультразвуковая&#13;
обработка докавитационными режимами приводит к существенному&#13;
(больше чем в 200 раз) увеличению плотности состояний на уровне Ферми, что вызывает не только количественные, но и качественные изменения вольтарадных зависимостей. В то же время влияние поля акустической кавитации деблокирует гельмгольцевскую ёмкость за счёт сильного уменьшения сопротивления области пространственного заряда в твёрдом теле. На основании полученных данных разработана электрохимическая система гибридного суперконденсатора с удельной ёмкостью 1100&#13;
Ф/г и удельной энергией 49 Втч/кг.
</description>
<dc:date>2013-01-01T00:00:00Z</dc:date>
</item>